NoticeYou can get Pro now by card, Apple Pay, Google Pay or bank transfer. We check each payment by hand and email your code. The free tools still work, and anyone who already has Pro keeps it. Get Pro or email me about instant checkout Meanwhile, most tools need no account; for the set print files, the brick tray and the videos, make a free, email-only account.
BrickalikePRO

Fixing warping and curling

Warping lifts the corners of flat parts and bends long ones. Heat and grip control it.

What you will see

What to try, in order

  1. Clean the plate with warm water and dish soap, and keep bare fingers off it afterwards.
  2. Bed temperature: textured PEI at about 55 to 60 °C for PLA; 70 to 80 °C for PETG (80 for small parts).
  3. Add a 3 to 5 mm brim.
  4. Slow first layer, about 25 mm/s.
  5. Keep drafts and cold air off the print; an enclosure helps.

Change one thing at a time and test with one piece, not a whole plate.

Good to know

Where we give numbers, they come from our own tests on a Bambu P1S with a 0.4 mm nozzle plus advice from other makers, and other printers need small adjustments. Our print settings page has the full table. Printed bricks are not toys: small parts, a choking hazard, not for children under 3.