NoticeYou can get Pro now by card, Apple Pay, Google Pay or bank transfer. We check each payment by hand and email your code. The free tools still work, and anyone who already has Pro keeps it. Get Pro or email me about instant checkout Meanwhile, most tools need no account; for the set print files, the brick tray and the videos, make a free, email-only account.
BrickalikePRO

Fixing small parts that will not stick

The smallest pieces have the least bed contact, so they let go first. These steps help.

What you will see

What to try, in order

  1. Slow first layer (about 25 mm/s) and a clean plate: warm water and dish soap, and no bare fingers on it afterwards.
  2. A 3 to 5 mm brim on the smallest pieces. Our Bambu files add it for you.
  3. PETG: bed at 75 to 80 °C for the first layer.
  4. Print only a few of them per plate if they keep letting go.

Change one thing at a time and test with one piece, not a whole plate.

Good to know

Where we give numbers, they come from our own tests on a Bambu P1S with a 0.4 mm nozzle plus advice from other makers, and other printers need small adjustments. Our print settings page has the full table. Printed bricks are not toys: small parts, a choking hazard, not for children under 3.